You might also like

Inclusions Phenomena at Steelmaking Sulphur, Phosphorus and Other Impurities One...
Steelmaking Technology  Steel Fabrication - Overview and Definition Steelmaking ...
Steel Bar Steel Bar - How It`s  Made ? Steel bar...
Forming Technology and Heat Treatments  Forming Technology and Heat Treatments There...
Grab This Widget
METALLURGY CORNER

Random Posts

  • Nickel Alloys
    Nickel is a chemical element, with the chemical symbol Ni and atomic number 28. It is a silvery-white lustrous metal wit...
  • Metallurgy Glossary
    Activity: A function of the chemical potential of a system. Alloy: A metallic substance that is composed of two or more...
  • Surface Hardening
    Surface hardening is the process of hardening the surface of a metal, often a low carbon steel, by infusing elements int...
  • Analysis of 316L Reducer Failure
    An 8" x 6", 316L stainless steel reducer was sent for failure analysis (Fig 1). It had been in service for 13 months whe...