Failure analysis is the process of collecting and analyzing data to determine the cause of a failure. It is an important discipline in many branches of manufacturing industry, such as the electronics industry, where it is a vital tool used in the development of new products and for the improvement of existing products.
Fatigue Failure
It relies on collecting failed components for subsequent examination of the cause or causes of failure using a wide array of methods, especially microscopy and spectroscopy. The NDT or nondestructive testing methods are valuable because the failed products are unaffected by analysis, so inspection always starts using these methods.
You might also like
| Analysis of 316L Reducer Failure Introduction: An 8" x 6", 316L stainless... | Shaft Bearing Failure Introduction: A bearing that had been in... | Bronze Bull Gear Failure Introduction : A bronze bull gear was sent... | Rider Roller Shaft Failure Introduction : A section of a failed "rider... |




Alloy Suppliers
Aluminum
Aluminum Extrusions
Copper-Brass-Bronze
Nickel
Magnets
Stainless Steel
Stainless Steel Tubing
Steel Service Centers
Titanium
Tungsten
Wire Rope