Do you know Martensite Transformation ?
Martensite is a body-centered tetragonal form of iron in which some carbon is dissolved. Martensite forms during quenching, when the face centered cubic lattice of austenite is distored into the body centered tetragonal structure without the loss of its contained carbon atoms into cementite and ferrite. Instead, the carbon is retained in the iron crystal structure, which is stretched slightly so that it is no longer cubic. Martensite is more or less ferrite supersaturated with carbon. Compare the grain size in the micrograph with tempered martensite.
The term “martensite” usually refers to a form of steel with a distinctive atomic structure created through a process called martensitic transformation. Martensite is made from austenite, a solid solution of iron with a small amount of carbon in it.
You might also like
| Martensite Formation What is Martensite ? Martensite is a hard,... | Iron Carbon Phase Diagram - Fe-Fe3C and T-T-T Diagram Iron Carbon Phase Diagram Iron-carbon... | Austenite - Gamma Iron Austenite - a Definition Austenite also... | Study Iron-Carbon (Fe-C) Phase Diagram Iron Carbon Phase Diagram A study of the... |




Alloy Suppliers
Aluminum
Aluminum Extrusions
Copper-Brass-Bronze
Nickel
Magnets
Stainless Steel
Stainless Steel Tubing
Steel Service Centers
Titanium
Tungsten
Wire Rope